  1. Product surface contamination

  Zinc alloy die castings not only need to ensure surface cleanliness before heat treatment, but also cannot be contaminated during the production process. If oil stains and corrosion occur in zinc alloy die castings before heat treatment, it will affect the effective adsorption of carbon during the treatment process. During the pre oxidation process, more oil fumes will be generated, which not only adhere to the surface of the product, hinder carburization, but also affect the stability of the furnace atmosphere.

  2. The influence of temperature

  The non-uniformity of temperature inside the furnace has a significant impact on zinc alloy die castings, and various unexpected situations during the production process can affect the uniformity of furnace temperature.

  Insufficient cooling

  The cooling performance and cleanliness of quenching oil can affect the quenching quality. The failure of the agitator and improper oil filling method can affect quenching and cooling, resulting in uneven hardness of zinc alloy die castings.

Read recommendations:

360 radiator aio

deep draw metal stamping manufacturers

aluminium corner profile 15mm

Aluminum furniture component

What items should die-casting mold factories inspect during mold acceptance.sheet metal enclosure fabrication

LEAVE A customers

lf you have any questions or comments, you can leave us a message and we will reply to you as soon as possible

Upload Files

Accepted file types: zip, rar, dxf, dwg, sldprt, slddrw, igs, stp, step, sat, x_t, cgr, ipt, par, jpg, jpeg, gif, png, pdf, xls, xlsx, doc, docx.
Maximum supported file is 5MB, for larger or multiple files please send email to Harvey@greenwayalu.com